Polymer Property : Tenacity = 0.177 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.177 - 0.212 N/tex
2.00 - 2.40 g/denier
ASTM D2256/ASTM D3822
NatureWorks® Ingeo™ 6400D Fiber Grade PLA
NatureWorks® PLA polymer 6400D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6400D is designed for extrusion into mechanically ..
Tenacity 0.177 - 0.265 N/tex
2.00 - 3.00 g/denier
LFL-09
Intercontinental Polymers 1140 Bicomponent HDPE/PET Fiber Type - 10 X 2 Inches
50/50 HDPE Sheath/PET Core. Luster: Semi-Dull. Finish: FDA Compliant.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, FDA-compliant products, non-wovens, filtrati..
Tenacity 0.177 N/tex
2.00 g/denier
Shakespeare AquaBattâ„¢ Staple fiber, denier 16
AquaBattâ„¢ is a uniquely designed fiber with deep grooves or channels along its longitudinal axis. These grooves provide unique features to the fiber that can serve as ducts to move fluid spont..