Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.406 N/tex | 4.60 g/denier | 2.3 lb. load |
Shakespeare WonderThread® M-7 diameter 0.006" Polyester Industrial Sewing Thread Applications: Specialty industrial sewing applications demanding polyester for:
1) Certifications that sewn goods are 100% polyester Chemical Resistance-polyester withstands low Ph, acidic enviro.. |
|||
Tenacity | 0.406 N/tex | 4.60 g/denier | Knot Strength |
UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=4.5) Specialties: Monomer containing type of 1022TApplications: Fishing net, Small size monofilament, Softness required applicationsInformation provided by UBE. |