Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.432 N/tex | 4.90 g/denier | 1.4 lb. load |
Shakespeare WhisperTouch® Ultra Soft low luster, TEX# 14 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |
|||
Tenacity | 0.432 N/tex | 4.90 g/denier | 0.87 lb. load |
Shakespeare WonderThread® SN-40 ultra soft TEX# 8 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |
|||
Tenacity | 0.432 N/tex | 4.90 g/denier | Line Strength |
UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=5) Specialties: Monomer containing type of 5034T, High softness Applications: Small-big size sport fishing line and long line (main line), Softness required applicationsInformation provided by UBE. |
|||
Tenacity | 0.432 N/tex | 4.90 g/denier | Straight test - filament yarn tested at 3 TPI, 10 inch gauge length and 60%/min extension rate. DuPont Test Method 12002 |
DuPont™ Nomex® 430 1600 Denier Aramid Yarn A high crystallinity natural filament yarn of NOMEX with higher strength and chemical resistance than staple spun yarns. Type 430 is used where the aesthetics and properties of a filament yarn are .. |