Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.794 N/tex | 9.00 g/denier | |
Kuraray Vectran® NT 1500/300 LCP Fiber  is a high-performance multifilament yarn spun from liquid crystal polymer (LCP).  fiber exhibits exceptional strength and rigidity. Pound for pound  fiber is five times stronger than steel an.. |
|||
Tenacity | 0.794 N/tex | 9.00 g/denier | |
Kuraray Vectran® UM 1500/300 LCP Fiber  is a high-performance multifilament yarn spun from liquid crystal polymer (LCP).  fiber exhibits exceptional strength and rigidity. Pound for pound  fiber is five times stronger than steel an.. |
|||
Tenacity | 0.794 N/tex | 9.00 g/denier | Tensile Modulus |
UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=6) Specialties: Monomer containing type of 7034T, High softness Applications: Small-big size sport fishing line and long line (branch line), Softness required applicationsInformation provided by UBE. |
|||
Tenacity | 0.794 N/tex | 9.00 g/denier | Tensile Modulus |
UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=6) Specialties: Monomer containing type of 5034T, High softness Applications: Small-big size sport fishing line and long line (main line), Softness required applicationsInformation provided by UBE. |
|||
Tenacity | 0.794 N/tex | 9.00 g/denier | Line Strength |
UBE 5033T Nylon 6/66 Monofilament (Drawing Ratio=6) Specialties: High viscosity Nylon 6/66 Copolymer, High transparent and tenacity, Higher drawing ratio can be achieved for superior line strengthApplications: Small-medium size sport fishing line Inf.. |