Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 1.94 N/tex | 22.0 g/denier | Tensile Modulus |
UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=4.5) Specialties: Medium viscosity Nylon 6/66 Copolymer, High knot strength (for Knot improvement), Softness is similar with 1022MT2 (At the heat setting of the net, higher shrink ratio may be expected t.. |
|||
Tenacity | 1.94 N/tex | 22.0 g/denier | Tensile Modulus |
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=6, Diameter 0.4 mm) Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic.. |