Polymer Property : Tenacity = 23.6 g/denier Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 2.08 N/tex
23.6 g/denier
DuPont™ Kevlar® 49 Aramid Fiber
1140 Denier; 768 Filaments. Kevlar® 49 is a high-modulus type used primarily in fiber optic cable, textile processing, plastic reinforcement, ropes, cables, and composites for marine sporting good..