Polymer Property : Tenacity = 3.00 g/denier Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.265 N/tex
3.00 g/denier
Technetics Group PLASTOLON™ PTFE Outdoor Fiber  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Tenacity 0.265 - 2.56 N/tex
3.00 - 29.0 g/denier
Average value: 0.723 N/tex Grade Count:25
Overview of materials for Nylon 6 Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatW..
Tenacity 0.265 - 0.574 N/tex
3.00 - 6.50 g/denier
Average value: 0.412 N/tex Grade Count:16
Overview of materials for Nylon 66 Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66 Fiber". Each property range of values reported is minimum and maximum values of appropriate Mat..
Tenacity 0.265 - 0.353 N/tex
3.00 - 4.00 g/denier
LFL-09
Intercontinental Polymers 1631 Bicomponent Polyester/PET Fiber Type - 4 Denier X 2 Inches
Semi-crystalline low melt polyester sheath/PET core. Luster: Semi-Dull. Finish: HydrophilicApplications of bicomponent polyester fiber: Absorbent products, FDA-compliant products, non-wovens, fi..
Tenacity 0.265 N/tex
3.00 g/denier
Shakespeare MX-200 PP Polypropylene Monofilament
Generally good chemical resistance. Good biological resistance.Information provided by Shakespeare Company.
Tenacity 0.265 N/tex
3.00 g/denier
Shakespeare Resistat® F9422 T040 Nylon 6 Monofilament
Resistat F9422, MERGE T040 is composed of forty filaments of conductive nylon 6 yarn. This yarn is twisted and heatset. Each filament has electrically conductive carbon suffused into the surface. ..
Tenacity 0.265 N/tex
3.00 g/denier
22.7 kg breaking load
Shakespeare Sanstat® CN125 .89mm Nylon 66 Monofilament
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by ..
Tenacity 0.265 N/tex
3.00 g/denier
Shakespeare Resistat® F9216 F040 Nylon 66 Monofilament
Resistat F2416, MERGE F040 is a nylon 6,6 multifilament yarn. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section with a coating th..
Tenacity 0.265 N/tex
3.00 g/denier
Shakespeare Resistat® F9222 B040 Nylon 6 Monofilament
Resistat F9222, MERGE B040 is a 22 denier per filament conductive nylon 6 tow. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section ..
Tenacity 0.265 N/tex
3.00 g/denier
Knot Strength
UBE 5034MTAX1 Nylon 6/66 Monofilament (Drawing Ratio=4.5)
Specialties: Excellent transparency and softness, Specially developed for very big size diameter (over 2mm in diameter)Applications: Big size diameter and high transparency required applications (ov..
Tenacity 0.265 N/tex
3.00 g/denier
Knot Strength
UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=5)
Specialties: Monomer containing type of 7034T, High softness Applications: Small-big size sport fishing line and long line (branch line), Softness required applicationsInformation provided by UBE.
Tenacity 0.265 N/tex
3.00 g/denier
Knot Strength
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=4.5, Diameter 2 mm)
Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic..
Tenacity 0.265 N/tex
3.00 g/denier
Technetics Group PLASTOLON™ PTFE Filtration Sewing Thread  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Tenacity 0.265 N/tex
3.00 g/denier
Shakespeare Resistat® F9116 A012 Nylon 66 Monofilament
Resistat F9116, MERGE A012 is a 16 denier per filament nylon 6,6 chopped fiber. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section..