Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.415 N/tex | 4.70 g/denier | 2.6 lb. load |
Shakespeare WonderThread® SN-40 ultra soft TEX# 27 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |
|||
Tenacity | 0.415 N/tex | 4.70 g/denier | Line Strength |
UBE 5034MTAX1 Nylon 6/66 Monofilament (Drawing Ratio=5) Specialties: Excellent transparency and softness, Specially developed for very big size diameter (over 2mm in diameter)Applications: Big size diameter and high transparency required applications (ov.. |