Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.416 N/tex | 4.71 g/denier | |
Shakespeare MX-229 PVDF Monofilament Outstanding resistance to weathering/UV exposure; outstanding chemical resistance; low surface energy; low COF; low moisture regain; inherent flame resistance.Information provided by Shakespeare Com.. |