Mechanical Properties Metric English Comments
Tenacity 0.221 - 0.441 N/tex
2.50 - 5.00 g/denier
ASTM D2256/ASTM D3822
NatureWorks® Ingeo™ 6201D Fiber Grade PLA
NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically ..
Tenacity 0.221 - 0.441 N/tex
2.50 - 5.00 g/denier
ASTM D2256/ASTM D3822
NatureWorks® Ingeo™ 6202D Fiber Grade PLA
NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically ..
Tenacity 0.221 - 0.441 N/tex
2.50 - 5.00 g/denier
ASTM D2256/ASTM D3822
NatureWorks® Ingeo™ 6204D Fiber Grade PLA
NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically ..
Tenacity 0.203 - 0.441 N/tex
2.30 - 5.00 g/denier
Average value: 0.308 N/tex Grade Count:8
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..