Tensile Creep Modulus, 1000 hours 890 MPa

@Strain <=0.500 %
129000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultramid® C3U BK 23079 PA6/66 FR (Conditioned)
Description: Injection-molding grade with improved flame retardance (free from halogens and phosphorus), used e.g. for impact resistant electrically insulating parts such as contact bases and plug c..
Tensile Creep Modulus, 1000 hours 890 MPa
129000 psi
ISO 899
BASF Ultramid® C3U PA66/6 (Conditioned)
Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance.