Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 920 MPa
133000 psi
Arkema Group Orgalloy® R 6600 Nylon 66 Alloy, Rigid Grade (Conditioned)
Rigid polyamide 6.6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema.