Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 18.0 - 310 MPa
2610 - 45000 psi
Average value: 99.2 MPa Grade Count:17
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..