Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 21.7457 - 83.3376 MPa

@Temperature 40.0 - 100 °C
3153.95 - 12087.1 psi

@Temperature 104 - 212 °F
Average value: 49.2 MPa Grade Count:1
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Tensile Creep Modulus, 1000 hours 21.7457 - 83.3376 MPa

@Pressure 0.500 - 7.00 MPa
3153.95 - 12087.1 psi

@Pressure 72.5 - 1020 psi
Average value: 49.2 MPa Grade Count:1
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..