Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 320 MPa

@Temperature 23.0 °C
46400 psi

@Temperature 73.4 °F
50%RH; ISO 899
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity..