Tensile Creep Modulus, 1000 hours 3180 MPa

@Time 3.60e+6 sec
461000 psi

@Time 1000 hour
50%RH; ISO 899-1
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im..
Tensile Creep Modulus, 1000 hours 3180 MPa

@Temperature 23.0 °C
461000 psi

@Temperature 73.4 °F
50%RH; ISO 899
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..