Polymer Property : Tensile Creep Modulus, 1000 hours = 4900 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 4900 MPa
711000 psi
ISO 899-1
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
Tensile Creep Modulus, 1000 hours 4900 MPa
711000 psi
ISO 899-1
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
Tensile Creep Modulus, 1000 hours 4900 MPa
711000 psi
cond.; ISO 899-1
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Tensile Creep Modulus, 1000 hours 4900 MPa
711000 psi
ISO 899-1
Lanxess Durethan® BKV 35 H2.0 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: automotive structures