Polymer Property : Tensile Creep Modulus, 1000 hours = 82700 psi
Polymer Property :
Tensile Creep Modulus, 1000 hours =
82700 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Creep Modulus, 1000 hours
570
MPa
82700
psi
Conditioned; ISO 889-1
Lanxess Durethan® B 40 SK 000000 Nylon 6
PA 6, non-reinforced, injection molding