Tensile Creep Modulus, 1000 hours 500 - 850 MPa
72500 - 123000 psi
Average value: 570 MPa Grade Count:5
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..