Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 6000 MPa

@Time 3.60e+6 sec
870000 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)  (Unverified Data**)
25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio..
Tensile Creep Modulus, 1000 hours 6000 MPa
870000 psi
ISO 899
BASF Ultrason S 2010 G4 20% Glass Filled PSU
Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Tensile Creep Modulus, 1000 hours 6000 MPa

@Time 3.60e+6 sec
870000 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal..
Tensile Creep Modulus, 1000 hours 6000 MPa

@Temperature 23.0 °C
870000 psi

@Temperature 73.4 °F
50%RH; ISO 899
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66  (Unverified Data**)
Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers