50% Modulus 0.000800 - 0.00150 GPa
0.116 - 0.218 ksi
DIN 53504 S2
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..