Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00750 GPa | 1.09 ksi | ISO 37 |
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00750 GPa | 1.09 ksi | ISO 37 |
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |