Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00760 GPa | 1.10 ksi | ASTM D412 |
Network Polymers Softflex® 9000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
50% Modulus | 0.00760 GPa | 1.10 ksi | ASTM D412 |
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |