Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00827 GPa | 1.20 ksi | ASTM D412 |
Lubrizol Estane® 2355-95AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Fuel resistant, extrusion laminate coatingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Dow Chemical.Lubrizol acquired the Pellethane.. |