Polymer Property : 50% Modulus = 0.120 ksi
Polymer Property :
50% Modulus =
0.120 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
50% Modulus
0.000830
GPa
0.120
ksi
ASTM D412
Network Polymers Softflex® 0470
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.