Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00510 GPa | 0.740 ksi | DIN 53504 |
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00510 GPa | 0.740 ksi | DIN 53504 |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00510 GPa | 0.740 ksi | DIN 53504 |
Lubrizol ESTANE® 5701F1 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.00510 GPa | 0.740 ksi | DIN 53504 |
Lubrizol ESTANE® 58437 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |