Mechanical Properties Metric English Comments
50% Modulus 0.00550 GPa
0.798 ksi
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2351-85AE elastomer is a polyether hybrid specialty polyurethane elastomer compound which combines excellent resistance to fuels and oils with good hydrolytic stability and high damping..
50% Modulus 0.00550 GPa
0.798 ksi
DIN 53504
Lubrizol ESTANE® T5213 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00550 GPa
0.798 ksi
DIN 53504
Lubrizol ESTANE® 58888 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..
50% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l..
50% Modulus 0.00550 GPa
0.798 ksi
DIN 53504
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..