Mechanical Properties Metric English Comments
50% Modulus 0.00870 GPa
1.26 ksi
DIN 53504
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00870 GPa
1.26 ksi
DIN 53504
Lubrizol ESTANE® 5715F2 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00870 GPa
1.26 ksi
DIN 53504
Lubrizol ESTANE® 58360 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..