Polymer Property : 50% Modulus = 2.057 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
50% Modulus 0.01418 GPa
2.057 ksi
ASTM D412
DuPont Performance Polymers Kalrez® Spectrum™ 0090 Fluoroelastomer
DuPont™ Kalrez® 0090 perfluoroelastomer parts deliver durable, reliable sealing solutions for applications requiring excellent rapid gas decompression (RGD) properties as well as high hardness and..