Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 121 MPa | 17500 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Hardness, H358/30 | 121 MPa | 17500 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Hardness, H358/30 | 121 MPa | 17500 psi | ISO 2039-1 |
Eurostar Staramide B40 PA6, Extrusion Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar. |