Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 122 MPa | 17700 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Hardness, H358/30 | 122 MPa | 17700 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 508 PBT (Europe-Africa-Middle East) VALOX 508 is a 30% glass reinforced PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, distributor caps, ignition rotors, voltage regulator.. |