Mechanical Properties Metric English Comments
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East)
LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics Lexan® ML3999 PC (Europe-Africa-Middle East)
LEXAN ML3999 is a medium viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics ULTEM ATX200F PEI (Europe-Africa-Middle East)
High flow Polyetherimide blend. Resin is RoHS compliant. UL94 V0 Listing. US FDA Food Contact compliant.
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics ULTEM ATX200R PEI Blend (Europe-Africa-Middle East)
High flow Polyetherimide blend with internal mold release. RoHS compliant. UL94 V0 Listing.
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East)
VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo..
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East)
VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors.
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East)
VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage.
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Europe-Africa-Middle East)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
Hardness, H358/30 125 MPa
18100 psi
ISO 2039-1
SABIC Innovative Plastics ULTEM ATX200 PEI Blend (Europe-Africa-Middle East)
High flow Polyetherimide blend. RoHS compliant, UL94 V0 Listing.