Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hardness, H358/30 126 MPa
18300 psi
ISO 2039-1
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East)
VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts.