Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 133 MPa | 19300 psi | ISO 2039-1 |
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |