Polymer Property : Hardness, H358/30 = 135 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hardness, H358/30 95.0 - 135 MPa
13800 - 19600 psi
Average value: 110 MPa Grade Count:3
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Hardness, H358/30 95.0 - 135 MPa
13800 - 19600 psi
Average value: 110 MPa Grade Count:3
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..