Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hardness, H358/30 = 15400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hardness, H358/30 106 MPa
15400 psi
ISO 2039-1
SABIC Innovative Plastics Cycoloy® C1000 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1000 is a PC+ABS blend developed with emphasis on excellent processing efficiency while maintaining good heat resistance and impact ductility. It is an excellent material choice for a wide ..
Hardness, H358/30 106 MPa
15400 psi
ISO 2039-1
SABIC Innovative Plastics GELOY HRA170 ASA (Europe-Africa-Middle East)
GELOY HRA170 is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour ..
Copyright © lookpolymers.com All Rights Reserved