Hardness, H358/30 95.0 - 115 MPa
13800 - 16700 psi
Average value: 104 MPa Grade Count:4
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..