Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 95.0 - 170 MPa | 13800 - 24700 psi | Average value: 145 MPa Grade Count:98 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |