Polymer Property : Hardness, H358/30 = 23200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hardness, H358/30 160 MPa
23200 psi
ISO 2039-1
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East)
LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re..
Hardness, H358/30 160 MPa
23200 psi
ISO 2039-1
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East)
Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors.
Hardness, H358/30 160 MPa
23200 psi
ISO 2039-1
SABIC Innovative Plastics ULTEM 2310EPR PEI
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Hardness, H358/30 160 MPa
23200 psi
ISO 2039-1
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Hardness, H358/30 160 MPa
23200 psi
ISO 2039-1
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing.
Hardness, H358/30 160 MPa
23200 psi
ISO 2039-1
SABIC Innovative Plastics ULTEM 2312 PEI (Europe-Africa-Middle East)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
Hardness, H358/30 160 MPa
23200 psi
ISO 2039-1
SABIC Innovative Plastics ULTEM AR9300 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution.
Hardness, H358/30 160 MPa
23200 psi
ISO 2039-1
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East)
VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd..