Polymer Property : Hardness, H358/30 = 234 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hardness, H358/30 234 MPa
33900 psi
ISO 2039-1
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..