Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 75.0 MPa | 10900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Hardness, H358/30 | 75.0 MPa | 10900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Hardness, H358/30 | 75.0 MPa | 10900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Hardness, H358/30 | 75.0 MPa | 10900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East) PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP.. |
|||
Hardness, H358/30 | 75.0 MPa | 10900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL PX2245 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2245 is a halogen free (according to VDE/DIN 472 part815) flame retardant material. The material fulfills the IEC 65 part 20.2 requirement at 1.6 mm thickness. |