Mechanical Properties Metric English Comments
Rupture Strength 68.9 MPa

@Temperature 871 °C,
Time 360000 sec
10000 psi

@Temperature 1600 °F,
Time 100 hour
Special Metals INCONEL® alloy 693
INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t..
Rupture Strength 69.0 MPa

@Temperature 871 °C,
Time 3.60e+6 sec
10000 psi

@Temperature 1600 °F,
Time 1000 hour
Sheet
Special Metals UDIMET® alloy 188 Cobalt-base Alloy
UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small ..
Rupture Strength 69.0 MPa

@Temperature 871 °C,
Time 3.60e+6 sec
10000 psi

@Temperature 1600 °F,
Time 1000 hour
Special Metals UDIMET® alloy D-979 Fe-Ni Alloy
UDIMET® alloy D-979 (UNS N09979) is an iron-nickel alloy designed for turbine disc applications at temperatures up to 1200-1400°F (649-760°C). Hardened by a complex precipitation of interm..