Mechanical Properties Metric English Comments
Rupture Strength 8.30 MPa

@Temperature 870 °C,
Time 3.60e+6 sec
1200 psi

@Temperature 1600 °F,
Time 1000 hour
Typical Stress-Rupture
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Rupture Strength 8.27 MPa

@Temperature 982 °C,
Time 3.60e+7 sec
1200 psi

@Temperature 1800 °F,
Time 10000 hour
Carlson C 800H Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists..