Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 10.0 MPa @Temperature 900 °C, Time 3.60e+7 sec |
1450 psi @Temperature 1650 °F, Time 10000 hour |
|
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Rupture Strength | 10.0 MPa @Temperature 900 °C, Time 3.60e+7 sec |
1450 psi @Temperature 1650 °F, Time 10000 hour |
|
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |