Mechanical Properties Metric English Comments
Rupture Strength 1035 MPa

@Temperature 650 °C,
Time 198000 sec
150100 psi

@Temperature 1200 °F,
Time 55.0 hour
Crucible Compaction Metals Rene 95 Nickel Based Superalloy
P/M Rene 95 is one of the highest strength alloys available for service in the range of 800°F to 1200°F (425°C to 650°C). The alloy also provides excellent high temperature creep resistance and..
Rupture Strength 1035 MPa

@Temperature 650 °C,
Time 324000 sec
150100 psi

@Temperature 1200 °F,
Time 90.0 hour
Crucible Compaction Metals Rene Supersolvus Rene 95 Nickel Based Superalloy
Supersolvus P/M Rene 95 is designed to provide even higher temperature creep resistance and stress rupture strength than subsolvus Rene 95. Chemistry is not modified. These properties are obtained..