Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 13.0 MPa @Temperature 900 °C, Time 3.60e+7 sec |
1890 psi @Temperature 1650 °F, Time 10000 hour |
|
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Rupture Strength | 13.0 MPa @Temperature 850 °C, Time 3.60e+7 sec |
1890 psi @Temperature 1560 °F, Time 10000 hour |
|
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Rupture Strength | 13.0 MPa @Temperature 850 °C, Time 3.60e+7 sec |
1890 psi @Temperature 1560 °F, Time 10000 hour |
|
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Rupture Strength | 13.0 MPa @Temperature 850 °C, Time 3.60e+7 sec |
1890 psi @Temperature 1560 °F, Time 10000 hour |
|
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |