Mechanical Properties Metric English Comments
Rupture Strength 14.0 MPa

@Temperature 850 °C,
Time 3.60e+7 sec
2030 psi

@Temperature 1560 °F,
Time 10000 hour
Outokumpu 4841 High Temperature Austenitic Stainless Steel
Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r..
Rupture Strength 14.0 MPa

@Temperature 870 °C,
Time 360000 sec
2030 psi

@Temperature 1600 °F,
Time 100 hour
Typical Stress-Rupture
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Rupture Strength 14.0 MPa

@Temperature 1000 °C,
Time 3.60e+7 sec
2030 psi

@Temperature 1830 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite Standard Nickel Alloy Castings, No. HR4
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..