Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Rupture Strength = 20600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 142 MPa

@Temperature 600 °C,
Time 3.60e+7 sec
20600 psi

@Temperature 1110 °F,
Time 10000 hour
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
Copyright © lookpolymers.com All Rights Reserved