Rupture Strength 231 MPa

@Temperature 650 °C,
Time 3.60e+7 sec
33500 psi

@Temperature 1200 °F,
Time 10000 hour
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..