Mechanical Properties Metric English Comments
Rupture Strength 165 MPa

@Temperature 815 °C,
Time 36000 sec
23900 psi

@Temperature 1500 °F,
Time 10.0 hour
Initial Stress
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Rupture Strength 165 MPa

@Temperature 760 °C,
Time 3.60e+6 sec
23900 psi

@Temperature 1400 °F,
Time 1000 hour
Sheet
Special Metals UDIMET® alloy 188 Cobalt-base Alloy
UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small ..
Rupture Strength 165 MPa

@Temperature 760 °C,
Time 3.60e+6 sec
23900 psi

@Temperature 1400 °F,
Time 1000 hour
Special Metals UDIMET® alloy L-605 Co-Cr-W-Ni Alloy
UDIMET® alloy L-605 (UNS R30605) is a solid solution strengthened cobalt-chromium-tungsten-nickel alloy with excellent high-temperature strength and excellent oxidation resistance to 2000°F (1093°..